Home > Knowledge > Content

Stainless Steel Chrome Plated Rod precision machining process analysis

Jan 14, 2023

(1) Stainless Steel Chrome Plated Rod is subjected to alternating loads in normal use, and there is a sealing device at φ50mm×770mm to rub its surface back and forth, so it requires high hardness and wear resistance.

The piston rod is made of 38CrMoALA material. After the φ50mm×770mm part is quenched and tempered and surface nitrided, the core hardness is 28~32HRC, the surface nitrided layer depth is 0.2~0.3mm, and the surface hardness is 62~65HRC. In this way, the piston rod has both certain toughness and good wear resistance.

(2) The structure of Stainless Steel Chrome Plated Rod is relatively simple, but its length-to-diameter ratio is large. It is a slender shaft part with poor rigidity. The tool rest is always used in the car to reduce the deformation of the workpiece during steam recovery processing, and the steady rest is used when processing the threads at both ends.

(3) When selecting the positioning datum, in order to ensure the coaxiality tolerance of the parts and the mutual position accuracy of each part, all processing procedures adopt two center holes for positioning, which conforms to the principle of unified datum.

(4) When grinding the outer circular surface, the workpiece is prone to yielding and elastic deformation, which affects the accuracy of the Stainless Steel Chrome Plated Rod. Therefore, the center hole should be repaired during processing, and the center hole should be kept clean. The tightness between the center hole and the gap should be appropriate, and good lubrication should be ensured. The general choice of grinding wheel: abrasive white corundum (WA), particle size 60#, medium hardness or medium, ceramic bond, and the width of the grinding wheel should be narrower to reduce the radial grinding force. Pay attention to the selection of grinding amount during processing. Especially the grinding depth should be small.

(5) When grinding φ50mm×770mm outer circle and 1:20 taper, the two processes must be carried out separately. When grinding 1:20 taper, the test piece must be ground first, and the workpiece can be formally ground only after the test piece is qualified.

The inspection of the 1:20 conical surface is to use the standard 1:20 ring gauge for color inspection, and the contact surface should not be less than 80%.

(6) In order to ensure the stability of the processing accuracy of Stainless Steel Chrome Plated Rod, manual alignment is not allowed during the whole process of processing.

(7) During nitriding treatment, the threaded parts, etc. should be protected by protective devices.

In order to increase the life of the piston rod and reduce the wear of the piston rod, 38CrMoAlA alloy structural steel is used for the blank.

Since the production type belongs to batch production, in order to improve production efficiency, it is advisable to adopt the free forging method to manufacture blanks. According to the technical requirements and assembly requirements of the piston rod, the center holes of the left and right end faces and both ends of the piston rod should be selected as the fine reference.

Many surfaces on a part can be machined with reference to both ends. It can avoid datum conversion error and follow the principle of datum unification.

The central axis at both ends is the design basis. Selecting the central axis as the benchmark can ensure the accuracy of the machining position of the surface and realize the coincidence of the design benchmark and the process benchmark. Since the finishing process of the two-axis surface requires a small and uniform allowance, it can be used as a reference.