The purpose of quenching and tempering treatment is to make the piston rod have comprehensive mechanical properties with good matching of strength, hardness, plasticity and toughness. The internal structure is uniform and fine tempered sorbite, which is well prepared for subsequent surface quenching. The long cylinder piston rod has a length of 3800-4200 and a diameter of Φ90-Φ110mm. Therefore, its heating equipment adopts a 150KW well-type resistance furnace or a 600KW suspended continuous resistance heating furnace. The temperature is controlled in upper and lower zones.
Heat treatment process parameters: 4 tubes are suspended in one furnace in a well-type furnace. The quenching heating temperature is 830±10°C. After 160 minutes of heat preservation, the tubes are discharged from the furnace and quenched in 2 times. 2 tubes are quenched each time. Cooling is carried out with circulating cooling water. During quenching and cooling, the tubes are moved up and down. Swing to ensure maximum uniform cooling, and when cooled to about 100°C (the rod emits steam but does not bubble), the water flows out into the well-type tempering furnace for tempering.
Then 4 pieces are heated at 550±10℃ at a time, kept warm for 190 minutes, tempered and then cooled with water. After the quenching and tempering treatment by the above process, the performance is unstable, the hardness fluctuates between 210-255HBS, and the upper, middle and lower hardness of the same piston rod also vary greatly. And sometimes the hardness of individual heats is unqualified or the strength is low and needs to be repaired. The quenching deformation is relatively large, which increases the difficulty of subsequent alignment and machining. Due to the poor hardenability of 45 steel, metallographic observation shows that its internal structure is not a single uniform tempered sorbite, but there are large pieces of free iron in its center, and some parts also have reticular iron and Widmanstatten structures. .
In order to solve the above problems, we use a suspended continuous heat treatment quenching and tempering furnace for quenching and heating. Each rack is equipped with 2 tubes. After heating and insulation, it is automatically quenched and one rack is output per beat to ensure uniform heating. Considering that the Ac3 temperature of 45 steel is 770-780°C, in order to refine the grains and reduce deformation as much as possible, we use a 790±10°C sub-temperature quenching process to refine the austenite grains and obtain fine and uniform austenite grains after quenching. Lath martensite to improve the strength and toughness of the piston rod.
In order to further reduce deformation and improve the uniformity of cooling of the quenching liquid, we add 5%-10% quenching additives to the tap water. During quenching, we also use a circulating water pump to force the cooling liquid to circulate. Tempering still uses 550±10℃ heating, and the beat is the same as that of quenching. After tempering, it is water-cooled to suppress the generation of the second type of temper brittleness. After the improvement of the above process, the internal structure is uniform and fine tempered sorbite, and the large or reticular ferrite and Widmanstatten structure are removed, and the hardness and strength are uniform and stable.
Quenching and tempering treatment of piston rod
Feb 13, 2024
Send Inquiry
Categories
Contact Us
- Tel: +8613861835411
- Email: andsonying@163.com
- Email: andsonying@wxboton.com
- Add: 2 Luxi Road, Yangshan Industrial Zone, Huishan District, Wuxi City, Jiangsu, China